In this study, denim fabrics four different constructions were sewn with two different sewing thread and two different stitch densities per centimeter using sewing needle 110/18 number, seam strength tests were performed to the fabrics. L & M sewability tests were performed to the same fabrics. Results of seam performance tests were compared with each other. When yarn thickness and density per centimeter increase, needle penetration force increase so sewability of fabrics is getting difficult. When stitch density per centimeter of fabrics in weft and warp directions increases, seam strength increases, too. When seam strength of the samples are compared; due to strength of the sewing thread Gral is higher than the sewing thread Epic seam strength of all samples sewn with the sewing thread Gral were higher than seam strength of the samples sewn with sewing thread Epic.
Bu çalışmada farklı konstrüksiyona sahip 4 denim kumaş, 110/18 numara dikiş iğnesi kullanılarak iki farklı dikiş ipliği ve iki farklı dikiş sıklığında standartlara uygun şekilde dikilmiş, dikiş mukavemeti testleri yapılmıştır. Aynı kumaşlara L&M dikilebilirlik testi yapılmış ve sonuçlar kıyaslanmıştır. Kumaşları oluşturan iplik sıklıkları ve kalınlıkları arttıkça dikilebilirlik kuvveti (gf) artmakta ve kumaşın dikilebilirliği zorlaşmaktadır. Atkı ve çözgü yönlerinde dikiş sıklığı arttıkça dikiş mukavemeti artmaktadır. Numunelerin dikiş mukavemetleri kıyaslandığında; Gral dikiş ipliğinin mukavemeti Epic dikiş ipliğinin mukavemetinden daha yüksek olduğu için; Gral dikiş ipliği ile dikilen tüm numunelerin dikiş mukavemetleri, Epic dikiş ipliği ile dikilenlere nazaran daha yüksek çıkmıştır.
Bölüm | Makaleler |
---|---|
Yazarlar | |
Yayımlanma Tarihi | 15 Haziran 2016 |
Yayımlandığı Sayı | Yıl 2016 Cilt: 31 Sayı: 1 |